Bi-component epoxy resin for mixing

RAYRESIN

Bi-component
epoxy resin for mixing
RAYRESIN

The two components – the base resin and hardener – should be mixed to trigger the polymerisation reaction, thus obtaining a composite with excellent bonding to metal, plastic and rubber components.

  • Polymerisation time: 40 min. a 20º C.
  • High insulation, dielectric strength: > 21 kV / mm.
  • Water absorption: : 0,8 % máx.
  • Hardness: 70 Shore D
  • IP 68 s/ IEC 529 standard

INSTALLATION SEQUENCE – Step 1

Step 2

Step 3